Some Issues and also Solutions of Exterior Wall Putty

Sep. 11, 2021


With the enhancement of individuals's needs on the high quality of structure design, numerous problems that occur throughout the painting procedure of outside wall putty are obtaining more and more focus. Here HPMC supplier LISTAL summarizes some troubles and remedies that conveniently happen in the building of outside wall surface putty, wishing to supply application experience for related markets.

606fbdf057006.jpg

Chemical Raw Material HPMC for Wll Putty


Pay interest to the rainy season


Throughout the rainy season, the putty is not dry as well as does not have sufficient architectural stamina to resist rainfall in all. The drenched putty layer will certainly exfoliate and the inner framework will certainly loosen up. If paint is used after drying as well as sanding, the layer will certainly likewise flake off after several wet and also dry cycles. It is essential to strictly keep an eye on the weather as well as to arrange the building and construction job effectively. If the putty is saturated by rain, it must be extensively examined, the drenched as well as loosened parts completely eliminated, and then partly putty fixed.


Weak point of putty on dry surfaces


A lot of outside putties are water-hardened products, as well as the stamina of the putty enhances in the presence of dampness. If the surface is as well completely dry, the putty does not have moisture, causing the hydration response to stop. When hydration is incomplete, the putty has reduced efficiency stamina and might even become seriously chalked. In this situation, water can be sprayed completely on the wall surface prior to building, or the putty can be scuffed and also brightened and after that watered intensively to maintain the putty in place to make sure that the putty that has actually quit moisturizing continues to moisturize to enhance its strength.


Concrete plaster wall surfaces peels


Putty has a high probability of flaking as well as peeling on freshly built concrete paste surfaces, which are extremely alkaline. When the humidity is high, calcium carbonate crystals with a very loose framework will form on the pure paste surface. Now, after the putty is scraped on the wall surface, the adhesion to the base is extremely weak, and also late peeling and also molting is unavoidable.

Attempt not to apply the putty on the cement paste surface, as the probability of troubles is high. If construction is needed, you need to wait for the basic elimination of alkali from the pure slurry surface area, then wait for the wall to dry prior to puttingty construction.


606fbdf057006.jpg


Little bubbles appear on the surface


Some exterior wall surfaces look dry externally, however have heavy wetness inside. When the moisture inside the wall surface is higher than the moisture of the air outside the wall surface, there will be a pressure distinction and also the dampness will spread outside the wall. If you scrape putty on the wall right now, due to the high viscosity of the outside putty, thick and also tiny bubbles will appear promptly.

In this case, thin batching as well as compaction can be accomplished initially to plug the vapor holes in the wall, and after that the second set can be scuffed immediately before the initial drying, which can dramatically decrease the variety of little bubbles.



In the construction of the project, it is required to understand the physical and chemical buildings of the putty as well as building laws scientifically to avoid related top quality mishaps under the facility of purely managing the on-site putty products to satisfy the indicators specified in the sector standards. 

Contact us for purchasing RDP and HPMC.